- 1897
- N
- HSSE 5% Co
- 9.75
- 9.75
- 89.00
- 43.00
- 135º
- Straight
- Professional
- 10
- Thermo-Resistant Alloys
- Stainless
- Steel
- Titanium Alloys
- Ferritic / Martensitic Stainless (<320 HB / <850 N/mm2)
- Treated / Heat-Treatable Alloyed Steel (300-400 HB / 1000-1300 N/mm2)
1.3 Treated/Heat-Treatable Alloyed Steel (300-400HB/850-1300N/mm2)  Feed (mm/rev.) 0,090    Cutting Speed (m/min.) 8-15 
2.2 Ferritic/Martensitic Stainless  (320HB/<850 N/mm2)              Feed (mm/rev.) 0,100    Cutting Speed (m/min.) 8-12 
4 Titanium Alloys                                                   Feed (mm/rev.) 0,080    Cutting Speed (m/min.) 10-15