04,90 mm-DRILL BIT UF IZAR STD. INTERNAL COOLANT 8XD X-ALCR
- IZAR Std.
- UF Grain
- X - AlCr
- 4.90
- 6.00
- 90.00
- 50.00
- 2
- 140º
- Flat
- 1
- Steel
- Stainless
- Cast Iron
- Thermo-Resistant Alloys
- Construction / Carbon Steel (<250 HB / <850 N/mm2)
- 45-55 HRC
- Alloyed Steel (<300 HB / <1000 N/mm2)
- Treated / Heat-Treatable Alloyed Steel (300-400 HB / 1000-1300 N/mm2)
- Materiales resistentes al desgaste (400-500 HB / 1300-1800 N/mm2)
- Austenitic Stainless (<250 HB / <850 N/mm2)
- Ferritic / Martensitic Stainless (<320 HB / <850 N/mm2)
- Cast Iron (<200 HB / <700 N/mm2)
- Cast Iron (200-300 HB / 700-1000 N/mm2)
- Aleaciones termorresistentes
- 0.190
- 100-120
- 0.160
- 90-110
- 0.090
- 75-95
- 0.050
- 0.060
- 60-70
- 0.080
- 50-65
- 0.145
- 125-150
- 0.135
- 90-110
- 0.060
P.1 Construction / Carbon Steel  (<250 HB/<850 N/mm2)               Feed (mm/rev.) 0.190       Cutting Speed (m/min.) 100-120 
P.2 Alloyed Steel  (<300 HB / <1000 N/mm2)                          Feed (mm/rev.) 0.160       Cutting Speed (m/min.) 90-110 
P.3 Treated/Heat-Treatable Alloyed Steel (300-400HB/1000-1300N/mm2)  Feed (mm/rev.)0.090       Cutting Speed (m/min.) 75-95 
P.4 Hardox (400-500 HB / 1300-1800 N/mm2)                           Feed (mm/rev.) 0.050       Cutting Speed (m/min.) 35-40 
M Austenitic Stainless  (<250 HB / <850 N/mm2)                    Feed (mm/rev.)   0.060       Cutting Speed (m/min.) 60-70 
P.5 Ferritic/Martensitic Stainless  (320HB/<850 N/mm2)              Feed (mm/rev.) 0.080       Cutting Speed (m/min.) 50-65 
K.1 Cast Iron  (<200 HB / <700 N/mm2)                               Feed (mm/rev.) 0.145       Cutting Speed (m/min.) 125-150 
K.2 Cast Iron  (200-300 HB / 700-1000 N/mm2)                        Feed (mm/rev.) 0.135       Cutting Speed (m/min.) 90-110 
S Heat-Resistant Alloys                                                   Feed (mm/0.060       Cutting Speed (m/min.) 35-50